45% iron silicon particles - particle size driven metallurgical reaction kinetics optimization schemeScientific Mechanisms and Advanced Applications1. Disruptive improvement of reaction efficiency by granularityDoubling specific surface area: The specific surface area of 1-5mm particles is 8-12 times that of bulk alloys, accelerating reaction kinetics;Deoxygenation speed comparison:Block shaped ferrosilicon: complete deoxidation takes 8-12 minutes;45% iron silicon particles: Deoxygenation can be completed in 3-5 minutes (efficiency increased by 150%).2. Addressing industry pain pointsDeoxygenation lag in refining furnace: particles dissolve instantly, avoiding component fluctuations caused by "block floating";Blockage of continuous casting nozzle: low aluminum content (Al ≤ 0.5%), reducing the risk of Al ₂ O3 inclusion deposition;Ultra low carbon steel aluminum control: replacing aluminum deoxidation to achieve [Al] ≤ 0.002%.
For more detailed technical details, please feel free to s…